Application field and production process of epoxy resin

Sep 18, 2025

Leave a message

ALow Viscosity Epoxy Resin System E175B/C035A/B

 

Main characteristics

E175B is a modified bisphenol A type epoxy resin, C035A/B is a modified amine epoxy resin curing agent. The mixed epoxy resin system composed of E175B and C035A/B has low viscosity and is suitable for RTM and vacuum introduction molding process. The room temperature curing performance is good, and the improvement of mechanical properties tends to be stable after curing at 25 ℃ for 7 days, and is similar to the test results after post-curing treatment.

Application areas

production of composite parts such as automotive products, rail transit, radar covers, drones, etc.

Performance parameters

 

E175B

C035A/ B

appearance color

colorless to yellow transparent liquid

yellow transparent liquid

mass mixing ratio

100

20

initial mixing viscosity( mPa·s,25 o C)

180

gel time(25 o C)

30-80min

curing Procedure

room temperature curing 24h +60 o C/8h

Tg( o C,DSC)

80-100 o C

 

1. Mechanical properties of resin casting body (room temperature curing for 7 days)

test Item
C035A
C035B
unit
tensile strength
72
71
MPa
tensile modulus
3.4
3.4
GPa
fracture elongation efficiency
4.4
5.0
%
bending Strength
111
110
MPa
flexural modulus
3.4
3.4
GPa

note: The mechanical properties are the test values at 25 ℃;

 

2. Resin casting mechanical properties (room temperature curing 1 day +60 ℃ 8 hours)

test Item
C035A
C035B
unit
tensile strength
68
68
MPa
tensile modulus
2.9
2.9
GPa
fracture elongation efficiency
10.4
9.5
%
bending Strength
105
107
MPa
flexural modulus
2.8
2.8
GPa

note: The mechanical properties are measured at 25°C; Post-curing releases the curing stress, so the modulus is degraded and the fracture productivity becomes longer.

 

Weigh the components A and B according to the mass mixing ratio, stir and mix well, and defoam if necessary.

Precautions

1. After the resin is used up as soon as possible to prevent the viscosity change from affecting the use.

2. The resin and curing agent should be placed in a cool and ventilated place for sealed preservation, and the use is prohibited when the properties change significantly.

 

info-400-400

 

Low Viscosity Epoxy Resin System E175B/C044/C045B

 

Basic Properties

E175B is a modified bisphenol A epoxy resin, and C044/C045B is a modified amine epoxy resin curing agent. The mixed epoxy resin system composed of E175B and C044/C045B has low viscosity and is suitable for RTM, vacuum introduction, pouring and other molding processes.

Product Features

1. Low viscosity, excellent impregnation characteristics, easy construction, easy operation;

2. Excellent mechanical properties, high toughness, good fatigue resistance;

3. The curing reaction heat is low, the resin mixture has a long pot life, and the preparation of thick products does not crack;

Application areas

production of composite parts such as automotive products, rail transit, radar covers, drones, etc.

Technical parameters

 

E175B

C044/C045B

appearance color

colorless to slightly yellow transparent liquid

colorless to light yellow transparent liquid

mass mixing ratio

100

25

initial mixing viscosity( mPa·s,25 o C)

200-300

gel time(25 o C)

90-600min

curing Procedure

room temperature curing 24h +60 o C/8h

Tg( o C,DSC)

80-100 o C

 

Performance table of resin casting body

test Item
typical value
test Method
tensile strength (MPa)
70-80
GB/T 2568
breaking elongation efficiency (%)
8-11
GB/T 2568
shore D hardness
80-85
GB/T 2411
glass transition temperature Tg(℃)
80-100
DSC(20K/min)

 

info-400-349

 

Medium viscosity epoxy resin system E720/C720

 

Main features

E720 is a modified medium viscosity epoxy resin, C720 is a modified low viscosity amine curing agent. The resin system composed of E720/C720 has the characteristics of curing at room temperature, which is suitable for manufacturing composite products by hand lay-up process without heating.

Application areas

production of composite parts such as automotive products, rail transit, radar covers, drones, etc.

Performance parameters

 

E720

C720

status

colorless to yellow transparent liquid

colorless to yellow transparent liquid

mixing mass ratio

100

20

initial mixing viscosity (mPa · s,25℃)

300

gel time (25℃)

30-50min

curing Procedure

room temperature curing 24h

 

Performance of resin casting body (after curing at room temperature for 7 days)

test Item
typical value
unit
tensile strength
72
MPa
tensile modulus
3.3
GPa
fracture elongation efficiency
6
%
bending Strength
115
MPa
flexural modulus
3.5
GPa

 

Construction recommendations

1. Do not use too much glue at a time. It is recommended to use a flat container with a larger bottom area and a smaller height to prevent heat accumulation and extend the pot life.

2. After the hand paste is completed, heat preservation measures (such as quilts, heat preservation blankets) or appropriate heating can be added to improve production efficiency.

 

info-400-332

 

Medium viscosity epoxy resin system E721/C721

 

Main features

E721 is a modified medium viscosity epoxy resin, C721 is a modified low viscosity amine curing agent. The resin system composed of E721/C721 has the characteristics of room temperature curing, low viscosity and high heat resistance temperature, which is suitable for the manufacture of high temperature resistant composite products and composite molds by hand paste process.

Application areas

production of composite parts such as automotive products, rail transit, radar covers, drones, etc.

Performance parameters

 

E721

C721

status

colorless to yellow transparent liquid

colorless to yellow transparent liquid

mixing mass ratio

100

20

initial mixing viscosity (mPa · s,25℃)

425

gel time (25℃)

30-50min

curing Procedure

60 ℃ 4-12H, post-curing 80-100 ℃ 4H

 

Performance of resin casting body (after curing at room temperature for 7 days)

test Item
typical value
unit
tensile strength
71
MPa
tensile modulus
3.0
GPa
fracture elongation efficiency
8.4
%
bending Strength
113
MPa
flexural modulus
3.0
GPa

 

Construction recommendations

1. Do not use too much glue at a time. It is recommended to use a flat container with a larger bottom area and a smaller height to prevent heat accumulation and extend the pot life.

2. After the hand paste is completed, heat preservation measures (such as quilts, heat preservation blankets) or appropriate heating can be added to improve production efficiency.

 

info-334-223

 

Epoxy resin system (low dielectric) E813/C813

 

Basic Properties

E813 is a modified bisphenol A type epoxy resin, and C813 is a modified acid anhydride curing agent. The epoxy resin system composed of E813 and C813 has the characteristics of medium and high temperature curing, high toughness and high strength, and is suitable for the preparation of high-strength composite products.

Application areas

production of composite parts such as automotive products, rail transit, radar covers, drones, etc.

Technical parameters

 

E813

C813

appearance color

light yellow transparent liquid

light yellow transparent liquid

mass mixing ratio

100

75

initial mixing viscosity( mPa·s,25 o C)

200-300

curing Procedure

curing system 100 ℃/2H +160 ℃/2H

Tg( o C,DSC)

120 o C

 

Performance table of resin casting body

test Item
typical value
test Method
tensile strength (MPa)
85
GB/T 2568
tensile modulus (GPa)
3.25
GB/T 2568
elongation at break (%)
7.9
GB/T 2568
compression strength (MPa)
150
GB/T 2569
bending strength (MPa)
140
GB/T 2570
flexural Modulus (GPa)
3.50
GB/T 2570
Send Inquiry